Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 6.02 GPa @Strain 1.53 %, Temperature 40.0 °C |
872 ksi @Strain 1.53 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Secant Modulus | 6.01 GPa @Strain 1.36981 %, Temperature 40.0 °C |
872 ksi @Strain 1.36981 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |