Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.47 GPa @Strain 2.90 %, Temperature 0.000 °C |
794 ksi @Strain 2.90 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |