Polymer Property : Secant Modulus = 595 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus 4.10 GPa

@Strain 1.40 %,
Temperature 23.0 °C
595 ksi

@Strain 1.40 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov..
Secant Modulus 4.10 GPa

@Strain 2.5045 %,
Temperature 23.0 °C
595 ksi

@Strain 2.5045 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&l