Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 2.25 GPa @Strain 1.89 %, Temperature 23.0 °C |
326 ksi @Strain 1.89 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l Unreinforced Medium Viscosity Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provi.. |
|||
Secant Modulus | 2.25 GPa @Strain 1.89 %, Temperature 23.0 °C |
326 ksi @Strain 1.89 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® S600F20UV WT660 Polybutylene Terephthalate (PBT) Unreinforced UV Stabilized Polybutylene Terephthalate Crastin S600F20 NC010 is an unreinforced lubricated medium viscosity polybutylene terephthalate resin for injection molding.Information provided.. |
|||
Secant Modulus | 2.25 GPa @Strain 2.40 %, Temperature 0.000 °C |
326 ksi @Strain 2.40 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100 BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Delrin 100 is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100 provides maximum toughness in the product line without modification and .. |
|||
Secant Modulus | 2.25 GPa @Strain 1.09 %, Temperature -40.0 °C |
326 ksi @Strain 1.09 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1600 NC010 Nylon 1010 Plasticized Toughened UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1600 NC010 is a renewable sourced Polyamide 1010 containing a minimum of 60% renewably sourced.. |