Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 9.30 GPa @Strain 0.0300 %, Temperature 0.000 °C |
1350 ksi @Strain 0.0300 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Secant Modulus | 9.34 GPa @Strain 1.76 %, Temperature 40.0 °C |
1350 ksi @Strain 1.76 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® RE5264 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 36% Glass Reinforced Polyethylene Terephthalate Rynite RE5264 NC010 is a 36% glass fiber reinforced color stabilized modified polyethylene terephthalate.Information provided by DuPont Performance Po.. |
|||
Secant Modulus | 9.32 GPa @Strain 0.100 %, Temperature 40.0 °C |
1350 ksi @Strain 0.100 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030GV NC010 Polytrimethylene Terephthalate (PTT) 30% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3030GV NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on pol.. |
|||
Secant Modulus | 9.29 GPa @Strain 0.210 %, Temperature 23.0 °C |
1350 ksi @Strain 0.210 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |
|||
Secant Modulus | 9.32 GPa @Strain 0.100 %, Temperature 40.0 °C |
1350 ksi @Strain 0.100 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Sorona® 3030G NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**)& 30% Glass Reinforced Polytrimethylene Terephthalate Sorona 3030G NC010 is a 30% glass reinforced PTT resin containing 25% renewably sourced ingredients by weight (37% based on polymer only) with goo.. |