Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.14 GPa @Strain 0.110 %, Temperature 0.000 °C |
1180 ksi @Strain 0.110 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935SUV BK593 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced UV Stabilized Polyethylene Terephthalate Rynite 935SUV BK593 is a 35% glass fiber /mineral reinforced UV stabilized modified polyethylene terephthalate resin with low warpage de.. |
|||
Secant Modulus | 8.12 GPa @Strain 2.60 %, Temperature -40.0 °C |
1180 ksi @Strain 2.60 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Secant Modulus | 8.15 GPa @Strain 0.520 %, Temperature 40.0 °C |
1180 ksi @Strain 0.520 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® GW520CS NC010 Polyethylene Terephthalate (PET) 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified pol.. |
|||
Secant Modulus | 8.11 GPa @Strain 1.26111 %, Temperature 23.0 °C |
1180 ksi @Strain 1.26111 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK615SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK615SF is a 30% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |