Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 8.36 GPa @Strain 1.52 %, Temperature 0.000 °C |
1210 ksi @Strain 1.52 %, Temperature 32.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30T NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T NC010 is a 30% glass fiber reinforced toughened polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |