Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 7.88 GPa @Strain 1.57 %, Temperature 23.0 °C |
1140 ksi @Strain 1.57 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |