Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.90 GPa @Strain 0.100 %, Temperature 100 °C |
856 ksi @Strain 0.100 %, Temperature 212 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G43HS1L BK104 Nylon 66
(Unverified Data**) 43% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 80G43HS1L BK104 is a 43% glass fiber reinforced heat stabilized black polyamide 66 resin with superior impact resistance.Information.. |
|||
Secant Modulus | 5.90 GPa @Strain 0.270 %, Temperature 23.0 °C |
856 ksi @Strain 0.270 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13HS1L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L NC010 is a 13% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |