Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 5.47 GPa @Strain 2.90 %, Temperature 0.000 °C |
794 ksi @Strain 2.90 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5330HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 30% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5330HF is a 30% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Secant Modulus | 5.47 GPa @Strain 0.670 %, Temperature 40.0 °C |
793 ksi @Strain 0.670 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |