Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 4.10 GPa @Strain 1.40 %, Temperature 23.0 °C |
595 ksi @Strain 1.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Secant Modulus | 4.10 GPa @Strain 2.5045 %, Temperature 23.0 °C |
595 ksi @Strain 2.5045 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK612SF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 15% Glass Reinforced Low Viscosity Polybutylene Terephthalate Developed for Super Fast Production Crastin SK612SF is a 15% glass fiber reinforced low viscosity polybutylene terephthalate for injecti.. |