Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 12.1 GPa @Strain 0.215 %, Temperature -20.0 °C |
1760 ksi @Strain 0.215 %, Temperature -4.00 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Secant Modulus | 12.1 GPa @Strain 0.700 %, Temperature -40.0 °C |
1760 ksi @Strain 0.700 %, Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® FR530 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.Information provided by DuPont .. |
|||
Secant Modulus | 12.1 GPa @Strain 1.52 %, Temperature 23.0 °C |
1750 ksi @Strain 1.52 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G45DH2 BK083 Polyphthalamide (PPA) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G45DH2 BK083 is a 45% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |
|||
Secant Modulus | 12.1 GPa @Strain 0.390 %, Temperature -40.0 °C |
1760 ksi @Strain 0.390 %, Temperature -40.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® EFE7374 BK416 Nylon 6
(Unverified Data**) 40% Glass Reinforced Toughened Polyamide 6 Zytel EFE7374 is a 40% fiber reinforced heat stabilized lubricated toughened polyamide 6 for injection molding. It has an improved impact resistance and ex.. |