Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Secant Modulus | 1.32 GPa @Strain 5.00 %, Temperature 23.0 °C |
191 ksi @Strain 5.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 300PE BK602 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 300PE BK602 (formerly DE20577) is a medium-high viscosity acetal homopolymer an enhanced version of Delrin 300CP with very low.. |
|||
Secant Modulus | 1.32 GPa @Strain 3.80 %, Temperature 0.000 °C |
192 ksi @Strain 3.80 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500AF Acetal (POM)
(Unverified Data**) 20% Teflon® Fiber Filled Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500AF is a medium viscosity acetal homopolymer resin containing 20% Teflon PTFE fibers. It is desi.. |
|||
Secant Modulus | 1.32 GPa @Strain 4.40 %, Temperature 23.0 °C |
191 ksi @Strain 4.40 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500CL NC010 Acetal (POM)
(Unverified Data**) Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500CL is a medium viscosity acetal homopolymer resin containing a chemical lubricant designed for low wear and fr.. |
|||
Secant Modulus | 1.32 GPa @Strain 6.00 %, Temperature 0.000 °C |
192 ksi @Strain 6.00 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500P NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved Processing Delrin 500P is a medium viscosity acetal homopolymer for injection molding. It has improved processing thermal stability good mechanical .. |