Polymer Property : Compressive Modulus = 400 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 1.21 - 2.76 GPa
175 - 400 ksi
Average value: 2.30 GPa Grade Count:6
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Compressive Modulus 1.52 - 2.76 GPa
220 - 400 ksi
Average value: 2.28 GPa Grade Count:20
Overview of materials for Nylon 6, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..