Polymer Property : Compressive Modulus = 8560 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 59.0 GPa

@Temperature 23.0 °C
8560 ksi

@Temperature 73.4 °F
prEN2580 Type B
Hexcel® HexPly® M48 180°C/356°F Curing Epoxy Matrix, M48/42%/G1094/1000
Fiber: T800H 6K, 5H Satin weave, 290 g/m2Information provided by HexCel