Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.03 - 35.0 GPa | 150 - 5080 ksi | Average value: 8.95 GPa Grade Count:5 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |