Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 53.0 GPa @Temperature 75.0 °C |
7690 ksi @Temperature 167 °F |
Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |
|||
Compressive Modulus | 53.0 GPa @Temperature 75.0 °C |
7690 ksi @Temperature 167 °F |
Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, TVR380/26% Fiber Information provided by HexCel |