Mechanical Properties Metric English Comments
Compressive Modulus 4.31 GPa
625 ksi
ASTM D695
Quadrant EPP Duratron® PEI U2300 Extruded 30% Glass Reinforced Polyetherimide (ASTM Product Data Sheet)
Compressive Modulus 4.31 - 6.47 GPa
625 - 938 ksi
Average value: 5.75 GPa Grade Count:3
Overview of materials for Polyetherimide (PEI), 30% Glass Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 30% Glass Fiber". Specific grades with glass content between 25% and 34% are included. E..