Polymer Property : Compressive Modulus = 2.8351 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Modulus 2.8351 GPa

@Temperature 23.0 °C
411.20 ksi

@Temperature 73.4 °F
ASTM D695
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Direct Formed  (Unverified Data**)
Information provided by Daelim H&L