Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.40 GPa | 203 ksi | ASTM D638 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Compressive Modulus | 1.40 GPa | 203 ksi | ASTM D638 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |