Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Modulus | 1.21 GPa | 175 ksi | ASTM D695 |
Quadrant EPP Proteus® PP Natural Co-Polymer Polypropylene (ASTM Product Data Sheet) |
|||
Compressive Modulus | 1.21 - 2.76 GPa | 175 - 400 ksi | Average value: 2.30 GPa Grade Count:6 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |
|||
Compressive Modulus | 1.21 GPa | 175 ksi | ASTM D695 |
Quadrant EPP Semitron® ESd 225, Extruded, Static Dissipative Acetal (ASTM Product Data Sheet) |