Polymer Property : Compressive Yield Strength = 26000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 28.0 - 179 MPa
4060 - 26000 psi
Average value: 120 MPa Grade Count:22
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum..
Compressive Yield Strength 68.9 - 179 MPa
10000 - 26000 psi
Average value: 140 MPa Grade Count:12
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Compressive Yield Strength 100 - 179 MPa
14500 - 26000 psi
Average value: 150 MPa Grade Count:10
Overview of materials for Nylon 610, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap..
Compressive Yield Strength 89.6 - 179 MPa
13000 - 26000 psi
Average value: 132 MPa Grade Count:27
Overview of materials for Nylon 612, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of ..
Compressive Yield Strength 138 - 179 MPa
20000 - 26000 psi
Average value: 153 MPa Grade Count:12
Overview of materials for Diallyl Phthalate (DAP), Cast, Mineral Filler
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP), Cast, Mineral Filler". Each property range of values reported is minimum and ma..
Compressive Yield Strength 159 - 179 MPa
23000 - 26000 psi
ASTM D695
Premix Premi-Glas® 1200H-24 Polyester SMC  (discontinued **)
Premi-Glas® 1200H-24 is a 24% fiberglass reinforced, thermoset, Sheet Molding Compound designed for applications where arc resistance and dielectric strength are required and UL 94 HB flame recogni..