Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 234 - 275 MPa
33900 - 39900 psi
Average value: 249 MPa Grade Count:6
Overview of materials for Phenolic, Resole, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..