Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 11.0 - 14.0 MPa | 1600 - 2030 psi | 1% deformation; ISO 604 |
Arkema Group VOLTALEF® 300 HD PCTFE VOLTALEF® 300 HD is a chlorotrifluoroethylene powder. Used for compression molding, very good flow, non-flammable. Information provided by Arkema Group |
|||
Compressive Yield Strength | 11.0 - 14.0 MPa | 1600 - 2030 psi | 1% deformation; ISO 604 |
Arkema Group VOLTALEF® 302 PCTFE VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group |
|||
Compressive Yield Strength | 4.00 - 14.0 MPa | 580 - 2030 psi | Average value: 10.0 MPa Grade Count:3 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |