Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 6.21 MPa @Strain 1.00 % |
901 psi @Strain 1.00 % |
ASTM D695 |
Saint-Gobain Fluoroloy® A09 High Performance Seal Material Extremely tough, long-wearing material; Excellent in water and water-based fluids, particularly suitable for abrasive media; Long wear life under severe conditions; Limited heat and chemical resista.. |