Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Yield Strength | 62.1 - 96.5 MPa | 9000 - 14000 psi | Average value: 86.9 MPa Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), PTFE/Glass-Fiber Filled". Each property range of values reported is minimum.. |
|||
Compressive Yield Strength | 62.1 - 172 MPa | 9000 - 24900 psi | Average value: 119 MPa Grade Count:14 |
Overview of materials for Nylon 6, Glass Filled, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Filled, Impact Grade". Each property range of values reported is minimum and maximum valu.. |
|||
Compressive Yield Strength | 62.1 - 68.9 MPa | 9000 - 10000 psi | Average value: 62.9 MPa Grade Count:8 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |
|||
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP1238 Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wetting to.. |
|||
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP1285HD-10 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP1285HD-14 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP1238 Black Acrylic / Epoxy Hybrid Adhesive Resinlab™ EP1238 Black is a two part acrylic / epoxy hybrid adhesive designed for bonding metals and plastics. It cures quickly at room temperature to a tough, semi-rigid material. It has good wett.. |
|||
Compressive Yield Strength | 62.1 MPa | 9000 psi | TM R050-38 |
Resinlab® EP1306 Acrylic / Epoxy Hybrid Adhesive EP1306 is a two part acrylic / epoxy hybrid adhesive utilizing a 50% weight loading of aluminum powder into both components. It cures quickly at room temperature to a tough, rigid polymer. It has go.. |