Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 500 MPa | 72500 psi | RT; Dry; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 37%/7781 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 500 MPa @Temperature 75.0 °C |
72500 psi @Temperature 167 °F |
Wet; DIN65380 |
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber Information provided by HexCel |
|||
Compressive Yield Strength | 500 MPa | 72500 psi | Warp, RT |
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26T/50%/7581 Glass Fabric 300 gsmInformation provided by HexCel |