Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.0140 MPa | 2.03 psi | at 25% deflection; ASTM D1056 |
Rogers Corporation Bisco™ BF-1000 Cellular Silicone Foam Soft, low compression set silicone foam often specified to meet safely-conscious requirements. UL recognized for flame retardance.Applications: Low closure-force gaskets and seals, Vibration and sh.. |