Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 131 - 172 MPa | 19000 - 25000 psi | Average value: 145 MPa Grade Count:3 |
Overview of materials for Nylon 66, 20% Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 20% Carbon Fiber Filled". Specific grades with carbon fiber content between 15% and 24% are in.. |