Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 107 - 574 MPa | 15500 - 83200 psi | Average value: 220 MPa Grade Count:9 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |