Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 6.89 - 350 MPa | 1000 - 50800 psi | Average value: 161 MPa Grade Count:21 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |