Mechanical Properties Metric English Comments
Compressive Yield Strength 96.5 - 148 MPa
14000 - 21500 psi
Average value: 114 MPa Grade Count:3
Overview of materials for Polycarbonate, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum a..
Compressive Yield Strength 33.0 - 148 MPa
4790 - 21500 psi
Average value: 87.0 MPa Grade Count:4
Overview of materials for Polyphenylene Sulfide (PPS), Unreinforced, Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Unreinforced, Extruded". Each property range of values reported is minimum ..