Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 75.8 MPa | 11000 psi | Mixed 2:1; TM R050-38 |
Resinlab® EP1215 Clear Unfilled Epoxy Structural Adhesive Resinlab™ EP1215 Clear is a two part unfilled epoxy structural adhesive designed for bonding applications requiring high strength and good impact resistance. It cures completely at room temperature.. |
|||
Compressive Yield Strength | 75.8 MPa | 11000 psi | |
Resinlab® EP691 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP 691 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting.. |
|||
Compressive Yield Strength | 75.8 - 103 MPa | 11000 - 15000 psi | Average value: 94.8 MPa Grade Count:4 |
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max.. |
|||
Compressive Yield Strength | 75.8 MPa | 11000 psi | ASTM D695 |
Devcon Combo Wear FC Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Compressive Yield Strength | 75.8 MPa | 11000 psi | ASTM D695 |
Devcon Wear Guard (Fine Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |
|||
Compressive Yield Strength | 75.8 MPa | 11000 psi | ASTM D695 |
Devcon Wear Guard (High Load) Epoxy Abrasion-Resistant SystemComments: PuttyData provided by Ellsworth Adhesives. |