Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 70.3 MPa | 10200 psi | ASTM D695 |
Devcon Plastic Steel® Liquid (B) Epoxy General Repair EpoxyComments: Steel-filled liquid epoxy can be cast over models for accurate detail reproduction when making holding fixtures, light-gauge forming dies and molds. Hardens in about a.. |