Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 50-3/AboCure 8012-2 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. High-Viscosity, like molasses; Dark Amber color. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 40-60 min. Industrial. Faster hardening.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 50-3/AboCure 8012-7 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Low-viscosity, like motor oil; Light Amber color; Combines lower viscosity with longer pot life. Shelf life is 12+ months.Processing: 2/1 ratio. Po.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 50-4/AboCure 50-22 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. High-Viscosity, like molasses; Light Amber color. A structural and dielectric standard. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life: 5.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 7802-1/AboCure 50-11 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Low-viscosity, Light Amber color. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 40-50 min. Lower viscosity and shorter pot life than Ab.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8008-6/AboCure 8008-6 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Colorless, "Liquid glass". Very low viscosity. Good color retention and lowest shrinkage. Unusually resistant to discoloration. Shelf life is 12+ m.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8012-3/AboCure 8012-3 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Low-viscosity, Heavy-duty, Dark Amber color. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 30 minutes.Corrosion Resistance Superior res.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-1/AboCure 8101-1 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Medium-viscosity, Light Amber color. Shelf life is 12+ months.Corrosion Resistance Best Abatron "VR" Epoxy for heat, solvent and chemical resistanc.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-2/AboCure 8101-2 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Lower-viscosity than AboCast 8101-1 for easier casting, encapsulating and potting. Shelf life is 12+ months.Processing: 2-1 ratio. Pot life: 2-3 hr.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-3/AboCure 8101-3 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Colorless, "Liquid glass". Superior thermal and chemical resistance, high hardness, lower exotherm permits larger castings. Shelf life is 12+ month.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-4/AboCure 8101-4 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Medium Amber liquid, Very low viscosity. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 20-30 minutes.Applications: wood restoration, co.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8101-8/AboCure 8101-8 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Tar filled, low-viscosity, black, plasticized resurfacing and patching compound. Shelf life is 12+ months.Processing: Pot-life: 1-2 hrs. 1/1 ratio... |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8102-1/AboCure 8102-1 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Medium viscosity; Amber. Heavy-duty industrial casting, filling and coating resin. Shelf life is 12+ months.Processing: 2/1 ratio. Pot life: 40-60.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 55-25/AboCure 55-25 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Paste form, Modified for minimum shrinkage and better heat transfer. Custom colors. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life: 1-2 .. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 7801-5/AboCure 7801-5 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Aluminum filled thixotropic paste. The most versatile of metal-filled pastes. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio. Li.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8012-4/AboCure 8012-4 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. A "Woodepox" version. neutral or colored; Low shrinkage. Shelf life is 12+ months.Processing: Pot life: 30-40 minutes. 1/1 ratio. Filled.Applicatio.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8012-5/AboCure 8012-5 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Aluminum filled putty, "plastic aluminum". non-shrinking, tough adhesive filler. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio... |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8012-6/AboCure 8012-6 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Iron filled putty, "plastic steel". non-shrinking, adhesive filler. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio.Applications:.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8101-6/AboCure 8101-6 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Vaseline like consistency, Light Amber color. Similar to AboCast 55-22. Best Abatron "VR" Epoxy for thermal, chemical, and solvent resistance. She.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8101-7/AboCure 8101-7 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Paste form, Modified for minimum shrinkage and maximum heat transfer. Similar to 55-25, but better rigidity, hardness, heat and chemical resistance... |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8101-9/AboCure 8101-9 Epoxy
(discontinued **) Data provided by the manufacturer, Abatron, Inc. Aluminum filled thixotropic paste. Highest heat, solvent and chemical resistance. Shelf life is 12+ months.Processing: Pot life: 1-2 hrs. 2/1 ratio.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 48-33/AboCure 48-33 Epoxy Data provided by the manufacturer, Abatron, Inc. Most versatile Abatron "VR" Epoxy thixotropic paste. White/black blend and other colors. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 55-22/AboCure 55-22 Epoxy Data provided by the manufacturer, Abatron, Inc. General purpose adhesive and patching paste for no-slump "invisible" repairs and bonds. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life: 1.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboWeld 8101-5/AboCure 8101-5 Epoxy Data provided by the manufacturer, Abatron, Inc. 5-minute epoxy thixotropic paste. Vaseline like consistency of 8012-9. Light Amber color. Shelf life is 12+ months.Processing: 1/1 ratio. Pot life:.. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | ASTM D695 |
Adell BS-10 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | ASTM D695 |
Adell BS-30 Nylon 6, General Purpose Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 62.0 MPa | 8990 psi | Typical value for Abatron "VR" Epoxies. |
Abatron AboCast 8012-9/AboCure 8012-9 Epoxy Data provided by the manufacturer, Abatron, Inc. 5-minute epoxy. Light Amber color, Medium viscosity. Not as brittle as conventional 5-minute epoxies. Fastest Abatron "VR" Epoxy with good physical .. |
|||
Compressive Yield Strength | 62.0 - 85.0 MPa | 8990 - 12300 psi | Average value: 74.2 MPa Grade Count:5 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |