Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 255 MPa | 37000 psi | ASTM D695 |
Adell AL-18 Nylon 66, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |
|||
Compressive Yield Strength | 255 MPa | 37000 psi | ASTM D695 |
Adell AL-38 Nylon 66, 40% Glass Reinforced; Mineral Filled Data provided by Adell Plastics, Inc. |