Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 185 MPa @Strain 10.0 %, Temperature 23.0 °C |
26800 psi @Strain 10.0 %, Temperature 73.4 °F |
EN ISO 604 |
Ensinger TECASINT 4011 Polyimide, Yellow (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |