Polymer Property : Compressive Yield Strength = 166 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 166 - 235 MPa
24100 - 34100 psi
Average value: 197 MPa Grade Count:10
Overview of materials for Phenolic, Novolac, Mineral/Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Fiber Filled". Each property range of values reported is minimum and maximum ..
Compressive Yield Strength 166 MPa
24100 psi
ASTM D695
Plenco 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok 308 is a two-stage, mineral and flock-filled phenolic molding compound designed to withstand the hostile environment of high abrasion and high tangential speed of engine pulleys. It is char..
Compressive Yield Strength 166 MPa
24100 psi
ASTM D695
Plenco 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Plaslok 309 is a two-stage, mineral and fiber-filled phenolic molding compound having excellent impact strength; and as such, is considered a good candidate for replacing chopped-fiber filled compou..
Compressive Yield Strength 166 MPa
24100 psi
ASTM D695
Plaslok 308 Black (COM) Mineral/Flock Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use. Plaslok 308 is a two-stage, mineral and flock..
Compressive Yield Strength 166 MPa
24100 psi
ASTM D695
Plaslok 309 Black (COM) Mineral/Fiber Filled Phenolic Molding Compound  (discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber..