Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Compressive Yield Strength = 14.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 14.0 MPa
2030 psi
at 5% nominal strain; ISO 604
Quadrant EPP Cestilene™ HD 1000 Polyethylene
Data provided by Quadrant Engineering Plastic Products for polymers in their European product line.
Compressive Yield Strength 14.0 - 110 MPa
2030 - 16000 psi
Average value: 60.5 MPa Grade Count:20
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Compressive Yield Strength 14.0 - 110 MPa
2030 - 16000 psi
Average value: 61.9 MPa Grade Count:7
Overview of materials for Acetal Homopolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values ..
Compressive Yield Strength 14.0 MPa
2030 psi
ASTM D395
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 35 pcf, MDI-based 2-Component Liquid System
0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience ..
Compressive Yield Strength 14.0 MPa

@Strain 1.00 %
2030 psi

@Strain 1.00 %
ISO 604
Manifattura Cattaneo PP-s Polypropylene
Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a.
Copyright © lookpolymers.com All Rights Reserved