Polymer Property : Compressive Yield Strength = 139 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 139 - 182 MPa
20200 - 26400 psi
Average value: 162 MPa Grade Count:5
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Compressive Yield Strength 139 - 213 MPa
20200 - 30900 psi
Average value: 175 MPa Grade Count:7
Overview of materials for Phenolic, Novolac, Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Flock Filled". Each property range of values reported is minimum and maximum values o..
Compressive Yield Strength 139 - 163 MPa
20200 - 23600 psi
Average value: 155 MPa Grade Count:3
Overview of materials for Phenolic, Resole, Mineral/Flock Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Resole, Mineral/Flock Filled". Each property range of values reported is minimum and maximum v..