Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 4.00 - 55.0 kN/m | 22.8 - 314 pli | Average value: 18.6 kN/m Grade Count:44 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |