Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® LBTW Polyester Film, 48 Gauge Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® OL2 Polyester Film, 50 Gauge Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge Product Description: Mylar® P25 is an uncoated, transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. S.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a co.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opp.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® RL31 Polyester Film, 50 Gauge Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl.. |
|||
Graves Tear Strength | 0.123 kN/m | 0.700 pli | ASTM D1004 |
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML.. |