Polymer Property : Graves Tear Strength = 0.123 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® CL Polyester Film, 100 Gauge
Mylar® CL is an exceptionally strong polyester film designed to package foods. Foods can be heated or cooked in this film at temperatures up to 400°F. Mylar® CL is commercially available in nomin..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® LBTW Polyester Film, 48 Gauge
Mylar® LBTW is an uncoated, transparent polyester film that has been corona treated on one side to provide superior wetting and adhesion of inks, primers, and adhesives. Mylar® LBTW is commerciall..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® OL2 Polyester Film, 50 Gauge
Product Description: Mylar® OL2 is a biaxially oriented polyester (OPET) film with an amorphous polyester heat seal layer. It is used as a heat sealable lidding film in packaging refrigerated and f..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® P25 Polyester Film, 50 Gauge
Product Description: Mylar® P25 is an uncoated, transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. S..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® P25T Polyester Film, 50 Gauge
Product Description: Mylar® P25T is a transparent polyester packaging film designed to be combined with a sealant layer, where the resulting structure will be shallow draw thermoformed. It has a co..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® RB52 Polyester Film, 50 Gauge
Product Description: Mylar® RB52 is a biaxially oriented polyester (OPET) film with an ethylene vinyl acetate (EVA) heat seal layer on one side and a polyvinylidene chloride (PVdC) layer on the opp..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® RL31 Polyester Film, 50 Gauge
Mylar® RL31 is a biaxially oriented polyester (OPET) with an ethylene vinyl acetate (EVA) heat seal layer. It is used as a heat sealable lidding film in packaging frozen and refrigerated foods. Myl..
Graves Tear Strength 0.123 kN/m
0.700 pli
ASTM D1004
DuPont Teijin Films Mylar® MLB Polyester Film, 48 Gauge
Product Description: Mylar® MLB is an uncoated, transparent, polyester film designed for use as a component of a lamination structure and may be suitable for use in medical applications. Mylar® ML..