Polymer Property : Flexural Strength = 12300 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 80.0 - 85.0 MPa
11600 - 12300 psi
ASTM D790
Prodways PLASTCure ABS 3650 3D Printing Polymer
Good chemical resistance. High transparency.Ideal for segments such like medical, electronic, aerospace and automotive markets that demand accurate RTV patterns, durable concept models, highly accur..
Flexural Strength 81.0 - 85.0 MPa
11700 - 12300 psi
ASTM D790
Prodways PLASTCure Cast 100 3D Printing Polymer
High reactivity and low viscosity. Excellent dimensional stability.Fulfills the high demands place on digital process chain.Information provided by Genistar.
Flexural Strength 75.0 - 85.0 MPa
10900 - 12300 psi
ASTM D790-03
Proto3000 Objet Digital Materials™ DM_7220 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide ..
Flexural Strength 80.0 - 85.0 MPa
11600 - 12300 psi
ASTM D790
Loxim 600 00HB Polycarbonate/Polybutylene Terephthalate
Information provided by Loxim Industries
Flexural Strength 82.0 - 85.0 MPa
11900 - 12300 psi
ASTM D790M
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin
DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts ..
Flexural Strength 65.0 - 85.0 MPa
9430 - 12300 psi
At Rupture; ISO 178
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..