Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 52.41 MPa | 7601 psi | ASTM D790 |
Lucent Polymers TPP-130 Polypropylene, Homopolymer, 30% Talc Filled Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc. |