Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 517 MPa | 75000 psi | Transverse Rupture |
Pacific Sintered Materials FCC-221-P Copper Steel Powdered Metal Applications:Medium strength mechanical componentsEquivalent MPIF Specification: FC-0205-35All information provided by Pacific Sintered Metals. |
|||
Flexural Strength | 517 MPa | 75000 psi | Transverse Rupture |
PSM Industries Pacific Sintered Metals Copper Steel FC-221-P Powdered Metal Medium strength mechanical components Equivalent MPIF Specification: FC-0205-35Information Provided by Pacific Sintered Metals, a division of PSM Industries |
|||
Flexural Strength | 517 MPa | 75000 psi | |
Pyrotek TS-109 Thermoset Electrical Insulation Product (Nema Grade: G-9) Glass reinforcement, Melamine Resin, Gray color. High mechanical strength, arc and heat resistance. Self-extinguishing.Information provided by Pyrotek. |
|||
Flexural Strength | 517 MPa | 75000 psi | |
Pyrotek TS-330 Thermoset Electrical Insulation Product Glass reinforcement, Polyester resin, Light Orange color. Very high compressive and flexural strength.Information provided by Pyrotek. |
|||
Flexural Strength | 517 MPa | 75000 psi | ASTM D790 |
Quantum Composites HTC-9593 55% Carbon Fiber Reinforced Bismaleimide SMC, High Temperature Composite HTC-9593 (127-51-5) is a 3K Pan Based Carbon Fiber reinforced Bismaleimide (BMI) ESC (Engineered Structural Composite) molding compound. It exhibits outstanding elevated temperature characteristics.. |
|||
Flexural Strength | 517 MPa | 75000 psi | Lengthwise; ASTM D790 |
G-10 Fiberglass Epoxy Laminate Sheet This glass-epoxy laminate is specified for its extremely high strength and high dimensional stability over temperature. G-10 is used for terminal boards, high humidity applications, electrical and e.. |
|||
Flexural Strength | 517 MPa | 75000 psi | ASTM F417 |
CoorsTek Pure SiC™ LR CVD Silicon Carbide, > 99.9995% Data Provided by the manufacturer, CoorsTek, Inc. |
|||
Flexural Strength | 517 MPa | 75000 psi | 90° stress angle |
Cytec Cyply® 1002 Epoxy Fiberglass Composite, Isotropic CYPLY® 1002 is a cured epoxy composite material based on a unique non-woven parallel filament construction. This type of construction minimizes filament stress abrasion that can shorten fatigue li.. |