Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 371 MPa | 53800 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RX12402 PA 66 LNP* Thermocomp* RX12402 is a compound based on PA66 containing 60% Glass Fiber. Added feature is Superior Flow. |