Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 34.4 MPa | 4990 psi | s.d. 1.7 MPa, specimen 2.49 cm wide (s.d. 0.02 cm), 0.21 cm thick (s.d.008 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C. |
Schmelzer Industries Curveil 220-20 Fiberglass Veil Good for curved applications - drapable and flexible. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. The 200 series contains a binder additive. .. |
|||
Flexural Strength | 34.4 MPa | 4990 psi | ASTM D790 |
Diamond Polymers NPP25-0103 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Flexural Strength | 34.4 MPa | 4990 psi | ASTM D790 |
Diamond Polymers NPP25-1111 CF15 Conductive Copolymer Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |