Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Schmelzer Industries Curveil 220-20 Fiberglass Veil

Category Ceramic , Glass , Glass Fiber , Other Engineering Material , Composite Fibers
Manufacturer Schmelzer Industries
Trade Name Curveil
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Schmelzer Industries Curveil 220-20 Fiberglass Veil.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Good for curved applications - drapable and flexible. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. The 200 series contains a binder additive. Data provided by the manufacturer, Schmelzer Industries.
Mechanical Properties Metric English Comments
Hardness, Barcol 32.7
32.7
Tensile Strength, Ultimate 19.45 MPa
2821 psi
s.d. 0.88 MPa, test specimen 1.21 cm wide (s.d. 0.003 cm), 0.19 cm thick (s.d. 0.008 cm)
Elongation at Break 0.57 %
0.57 %
Elongation at max. load, 0.54%
Modulus of Elasticity 4.03 GPa
585 ksi
std. dev. 0.30 GPa
Flexural Strength 34.4 MPa
4990 psi
s.d. 1.7 MPa, specimen 2.49 cm wide (s.d. 0.02 cm), 0.21 cm thick (s.d.008 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Flexural Modulus 3.30 GPa
479 ksi
Tangent