Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 200 MPa | 29000 psi | |
Plastcom SLOVASTER® B/E GF 30 PBT, 30% glass fibre FeaturesPBT/PET for injection moulding, chemically reinforced with 30% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and ben.. |
|||
Flexural Strength | <= 200 MPa | <= 29000 psi | ISO 178 |
Polykemi AB SCANAMID 66 A12^ F20 FR6 Nylon 66, Glass Fiber Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Flexural Strength | 200 MPa @Temperature -40.0 °C |
29000 psi @Temperature -40.0 °F |
ASTM D790 |
Penn Fibre Pennite® 4512 Nylon 6, 12% Glass Fiber Reinforced (PA6) PENNITE® 4512 is a 12% glass fiber reinforced, black pigmented, thermally modified, type 6 nylon, available in sheets and rolls for high performance thermoforming and fabrication applications. PENN.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ASTM D-790 |
Glastic T-160 Fiberglass-Reinforced Polyester Laminate Grade T-160 is a new, high-strength, heat-resistant laminate. This highly creep-resistant material is excellent for applications where electrically insulating materials are subject to physical load.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ISO 178 |
Solvay TECHNYL® A 21T2 V25 PA66, 25% glass fiber, DRY Description: Flame retardant polyamide 66, reinforced with 25% of glass fiber, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North AmericaProduct Appl.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ISO 178 |
Solvay Specialty Polymers Ryton® R-4-02 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Flexural Strength | 200 MPa | 29000 psi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Valox® 4631 PBT (Europe-Africa-Middle East) VALOX 4631 is a 30% glass reinforced, flame retarded PBT injection moulding resin with good electrical properties and excellent mechanical properties. |
|||
Flexural Strength | 200 MPa | 29000 psi | GB/T 9341-2008 |
Sichuan Deyang Haton® hGC51 PPS / AE Polyphenylene Sulfide Injection molding, conductiveInformation provided by Sichuan Deyang Chemical Co., LTD |
|||
Flexural Strength | 200 - 350 MPa | 29000 - 50800 psi | |
Sinotek Materials CFC Carbon Heat Insulation Material Information provided by Sinotek |
|||
Flexural Strength | 200 MPa | 29000 psi | ISO 178; ASTM D790 |
Styron DLGF9411.00 Polypropylene Overview: DLGF 9400.00 is a 40% long glass fiber reinforced grade with good flow properties. The glass fibers (12 mm length) are coupled to the polypropylene matrix resulting in high stiffness and s.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ISO 178 |
Solvay Specialty Polymers Ryton® XE5030BL Polyphenylene Sulfide Alloy (PPS Alloy), 30% Glass Fiber Ryton® XE5030BL 30% glass fiber reinforced polyphenylene sulfide alloy compound provides high ductility and impact resistance along with good thermal stability.Features: Ductile; Good Thermal Sta.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ASTM D790 |
Sumitomo Bakelite Sumikon® PM-9501 Glass-Filled Phenolic, Injection Grade Sumikon PM-9501 is a two stage glass fiber and mineral filled black phenolic special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ASTM D790 |
Chase Plastics CP Pryme® N120GL (DAM) Nylon 6, 20% Glass Fiber Reinforced, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Strength | 200 MPa | 29000 psi | At Rupture; ISO 178 |
Vyncolit X613 Novolac Phenolic Glass fiber filled phenolic molding compound with excellent mechanical and thermal properties. UL listed.USES: Solenoid covers or automotive under-bonnet applications such as: water pumps, impeller.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ASTM-D790 |
Polyram Polytron P50B03 Copolymer Polypropylene, Chemically Coupled 50% Long Glass Fiber A CHEMICALLY COUPLED 50% LONG GLASS FIBER REINFORCED BLACK POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteristi.. |
|||
Flexural Strength | 200 MPa | 29000 psi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® 70G33HS1L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G33HS1L NC010 is a 33% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perfor.. |
|||
Flexural Strength | 200 MPa | 29000 psi | 2 mm/min; ISO 178 |
Eurostar Staramide BG4H PA6, 20% Glass Filled, Injection Molded BG4H is a Heat Stabilized, 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Flexural Strength | 200 MPa | 29000 psi | ASTM D790 |
Aclo Accutech Polycarbonate POL051G30L Glass Reinforced |
|||
Flexural Strength | 200 MPa | 29000 psi | ISO 178 |
Ascend Performance Materials Vydyne® R533H BK10A0 Nylon 66, 33% Glass Reinforced, Conditioned Vydyne® R533H BK10A0 is 33% glass-fiber reinforced, hydrolysis-resistant, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical propertie.. |
|||
Flexural Strength | 200 MPa | 29000 psi | dry; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Flexural Strength | 200 MPa | 29000 psi | ASTM D790 |
Beijing Chemical Industry KAIFA® MN201-G25 Nylon 66 Resin 25% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Strength | 200 MPa | 29000 psi | |
Lehmann & Voss LUVOCOM® 1301/CF/15/TF/5-1 PPS, linear, with carbon fiber and PTFE Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w.. |